Some thoughts about galavic corrosion and its prevention in carbon composites with metal inserts are presented. A simple method to control if a pice is endangered of galvanic corrosion is shown. We exemplifly with #hortenmicrolight's control levers, which are a carbon and PVCfoam sandwich with usual steel bearings.