10 types of metal casting defects, what went wrong, and what you and your supplier can do to fix it together.
1. Gas hole porosity
2. Hydrogen gas porosity
3. Inclusions & sand inclusions
4. Shrinkage
5. Bent or twisted
6. Misrun or short pour
7. Crack
8. Rough surface finish
9. Flash
10. Parting line shift or mold misalignment
..................................
Batesville Products is a permanent mold aluminum casting, machining, and polishing foundry in Lawrenceburg, IN. Serving 70+ industries since 1946. Learn more here: https://batesvilleproducts.com/
....................................
#foundry #metalcasting #manufacturing #manufacturer #aluminum #aluminumcasting #permanentmold
CHAPTERS
00:0000:44 Intro
00:4403:14 Gas Hole Porosity
03:1405:36 Hydrogen Gas Porosity
05:3606:20 Inclusions
06:2008:00 Part Design Defects
08:0010:30 Mold Design Defects
10:3011:31 Mold Maintenance Defects
11:3112:49 Supplier Related Defects
12:4913:07 Outro